FIELD: dehydration of pulp of calcium hypochlorite. SUBSTANCE: method is carried out by adding of reduction agent which takes place at uninterrupted mixing. Solution of technical lignosulfonate having concentration 90.0-95.0 g/l is used as said reduction agent. During said reduction ratio of reduction agent and active chlorine is maintained within (1.3-1.5):1 g/g. Wastes of production of sulfite cellulose being diluted at ratio of water and technical lignosulfonate (4.6-5.0):1 are used as mentioned above solution of technical lignosulfonate. EFFECT: improved efficiency. 4 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF MAGNESIUM AND CHLORINE BY ELECTROLYSIS OF ANHYDROUS CHLORIDES | 2001 |
|
RU2209258C1 |
METHOD OF DECONTAMINATING CALCIUM HYPOCHLORITE PULP | 2018 |
|
RU2687455C1 |
METHOD FOR DEHYDRATING PUMP OF CALCIUM HYPOCHLORITE | 0 |
|
SU998326A1 |
METHOD OF PRODUCING CALCIUM SULPHATE DIHYDRATE | 2010 |
|
RU2437835C1 |
METHOD OF DETOXICATION AND UTILIZATION OF HYPOCHLORITE SOLUTIONS | 1996 |
|
RU2091327C1 |
METHOD OF TREATING TITANIUM-MAGNESIUM PRODUCTION EFFLUENT GASES | 2001 |
|
RU2201792C2 |
METHOD FOR NEUTRALIZING HYPOCHLORITE CALCIUM PULP | 2016 |
|
RU2636082C1 |
MAGNESIUM-CONTAINING ORE PROCESSING METHOD | 2004 |
|
RU2259320C1 |
METHOD OF CLEANING MAGNESIUM PRODUCTION EMISSION GASES | 1999 |
|
RU2169037C1 |
METHOD OF CATALYTIC DECOMPOSITION OF HYPOCHLORITE | 2001 |
|
RU2203850C2 |
Authors
Dates
1997-02-20—Published
1994-09-16—Filed