FIELD: textile industry. SUBSTANCE: aldehyde-containing polyvinyl-alcohol fibers are mixed with freshly shaped polyvinyl-alcohol fibers in proportion from 1: 1 to 1:3 and then treated with IR rays for 40-80 s. Mixed material is fit for manufacturing dressing and hygienic means with high moisture absorption. EFFECT: improved consumer's' qualify. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF TREATMENT OF FRESHLY FORMED POLYVINYLALCOHOL FIBER | 1996 |
|
RU2103426C1 |
METHOD FOR PRODUCING HYDROPHILIC POLYACRYLONITRILE FILAMENTS | 1998 |
|
RU2146312C1 |
METHOD FOR PRODUCING NUTRIENT MEDIUM FOR GROWING OF MUSHROOM BIOMASS | 1996 |
|
RU2125364C1 |
METHOD OF PREPARING PURIFIED INFLUENZA VIRUS BIOMASS | 1993 |
|
RU2057804C1 |
METHOD OF MANUFACTURING VISCOSE FIBERS | 1994 |
|
RU2096536C1 |
THREE-DIMENSIONAL NONWOVEN MATERIAL | 1994 |
|
RU2093626C1 |
METHOD OF MANUFACTURING ION-EXCHANGE FIBER | 2000 |
|
RU2194809C2 |
METHOD OF PREPARING CELLULOSE SOLUTIONS | 2000 |
|
RU2184750C2 |
METHOD OF SORPTION EXTRACTION OF CESIUM FROM NATURAL AND TECHNOLOGICAL WATERS | 1993 |
|
RU2065629C1 |
HIGH-BULK YARN | 1997 |
|
RU2128739C1 |
Authors
Dates
1997-03-27—Published
1994-01-26—Filed