FIELD: mineral dressing. SUBSTANCE: ore is crushed to particle size 0.1 mm and subjected to autoclave leaching of manganese with saturated calcium chloride solution at ratio 1:(3.0-3.5) followed by heating slurry for 0.5-1.0 h and pumping it through battery of autoclaves heated to 200-220 C. Then slurry is supplemented with 40-65% (based on solid weight) calcium chloride and such amount of ferrous chloride providing its concentration in solution 2.0-2.5%. Slurry is once again pumped through autoclave battery at 200-220 C for 0.5-1.0 h, supplemented with more ferrous chloride to its concentration in solution 2.0-2.5% and pumped through autoclave battery at 240-260, cooled to 90-100 C, freed from solids, and manganese compounds are precipitated and calcined. EFFECT: enhanced efficiency of process.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR EXTRACTION OF MANGANESE FROM MANGANESE FERROALLOY PRODUCTION WASTES | 1993 |
|
RU2057195C1 |
METHOD FOR CHEMICAL CONCENTRATION OF OXIDE-BEARING MANGANESE ORES | 1993 |
|
RU2038396C1 |
METHOD OF MANUFACTURING BRIQUETS FOR DIRECTLY ALLOYING STEEL WITH MANGANESE | 1994 |
|
RU2086675C1 |
MANGANESE ORE PROCESSING METHOD | 2001 |
|
RU2175991C1 |
BRIQUETTE FOR DIRECT ALLOYING OF STEEL | 1994 |
|
RU2090625C1 |
METHOD OF PROCESSING MANGANESE CARBONATE ORE | 2010 |
|
RU2441085C1 |
METHOD FOR CHEMICAL ENRICHMENT OF POLYMETALLIC MANGANESE CONTAINING ORE | 2015 |
|
RU2583224C1 |
METHOD OF CLEARANCE OF BEARING HEAVY NON-FERROUS METALS SULFATE SOLUTIONS FROM IRON | 1993 |
|
RU2068007C1 |
METHOD FOR INTEGRATED TREATMENT OF MANGANESE CARBONATE-OXIDE ORE | 2013 |
|
RU2539885C1 |
METHOD OF PROCESSING MANGANESE-CONTAINING MATERIALS | 1999 |
|
RU2172358C2 |
Authors
Dates
1997-09-20—Published
1993-02-11—Filed