FIELD: steelmaking. SUBSTANCE: method consists in introducing ferroalloys into ladle, tapping metal and slag, balancing blowoff with neutral gas, ladle sampling, introducing ferroalloys correcting chemical analysis of metal, and final blowoff. According to invention, if thickness of slag layer in ladle is not larger than 200 mm and weight of ferroalloys introduced into ladle before tapping smelt is not higher than 700 kg, balancing blowoff is performed for 2 min and introducing ferroalloys correcting chemical analysis of metal and final blowoff are performed not earlier than when 70% of time metal being in ladle from the beginning of tapping to the beginning of casting is expired. EFFECT: enhanced efficiency of process. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF STEEL PRODUCTION IN ARC FURNACES | 1995 |
|
RU2096489C1 |
METHOD OF SMELTING STEEL IN ARC FURNACES | 1995 |
|
RU2094479C1 |
METHOD OF PRODUCING BORON-CONTAINING STEEL | 2011 |
|
RU2492248C2 |
MANUFACTURING METHOD OF BORON STEEL | 2008 |
|
RU2382086C1 |
METHOD OF STEEL PRODUCTION | 2008 |
|
RU2374330C1 |
METHOD FOR OFF-FURNACE STEEL TREATMENT | 2015 |
|
RU2607877C2 |
METHOD OF MICRO-ALLOYING OF STEEL WITH NITROGEN | 2004 |
|
RU2266338C2 |
PROCEDURE FOR PRODUCTION OF HIGH CARBON ROD | 2008 |
|
RU2389802C2 |
LOW-SILICON STEEL PRODUCTION METHOD | 2023 |
|
RU2818526C1 |
METHOD OF PRODUCED HOT-ROLLED SHEET | 2010 |
|
RU2410174C1 |
Authors
Dates
1997-10-27—Published
1995-06-19—Filed