FIELD: ferrous metallurgy. SUBSTANCE: charge contains (in wt %): coke, 10-40; metal waste, 6-30; rolled briquettes of worked out contact mass from chemical production, 0.3-20.0; and quartzite, the balance. EFFECT: reduced cost due to utilizing waste components. 3 cl, 1 tbl