FIELD: biotechnology. SUBSTANCE: porous collagen-containing material to be frozen preliminary is thawed out, treated with an alkaline agent aqueous solution at pH 10-12 and 0.1-1.0-% formaldehyde solution, washed out to neutral medium reaction, pressed out nonbound moisture and dried at 20-60 C. If necessary, before final drying material is impregnated with solution of medicinal and/or antiseptic agent and pressing at 40-100 kg/cm2. EFFECT: improved method of preparing, improved quality of material, broadened pattern of the porous collagen-containing materials. 2 cl, 10 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING POROUS FIBROUS MATERIAL | 1995 |
|
RU2116350C1 |
METHOD OF POROUS PROTEIN TEXTURATE PRODUCING | 1997 |
|
RU2118495C1 |
METHOD OF VIRUS CONCENTRATING | 1997 |
|
RU2130069C1 |
METHOD OF PRODUCING POROUS COLLAGEN MATERIAL | 2018 |
|
RU2704248C1 |
PROCESS FOR PREPARING COLLAGEN SPONGE | 1993 |
|
RU2039766C1 |
COMPOSITION AS ANTIBACTERIAL AGENT, METHOD FOR PRODUCTION OF MATERIAL ON ITS BASIS AND MACROPOROUS ANTIBACTERIAL MATERIAL BASED ON THIS COMPOSITION | 2009 |
|
RU2404781C1 |
METHOD OF PREPARING POROUS COLLAGEN MATERIAL | 1993 |
|
RU2061051C1 |
PROCESS FOR PREPARING COLLAGEN CONTAINING MATERIAL | 1992 |
|
RU2018540C1 |
METHOD OF STERILE COLLAGEN BASE "FIBRICOLL" PREPARING | 1996 |
|
RU2118168C1 |
BIOCATALYST AND METHOD FOR ITS PREPARING | 2002 |
|
RU2233327C2 |
Authors
Dates
1998-08-10—Published
1995-06-15—Filed