FIELD: corrosion protection. SUBSTANCE: corrosion from heat carrier is prevented by successively affecting surfaces with light metal nitrates at 90-100 C and with nitrites of these metals at ambient temperature for 3-4 h each time and with obligatory washing after each action. EFFECT: simplified operation. 3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ACCELERATED TESTS OF SHIP CADMIUM ELECTRODEPOSITED COATINGS | 1991 |
|
RU2006828C1 |
METHOD OF PASSIVATION OF EQUIPMENT AND ARTICLES MADE FROM PEARLITE STEELS | 2000 |
|
RU2228388C2 |
METHOD OF ACCELERATED NICKEL COATING TEST | 1994 |
|
RU2092812C1 |
METHOD OF MANUFACTURE OF MAGNETITE ANODES FOR CATHODE CORROSION PROTECTION SYSTEM | 1999 |
|
RU2178010C2 |
METHOD FOR PROTECTING PEARLITE STEELS AGAINST CORROSION | 2000 |
|
RU2182192C1 |
METHOD FOR DECONTAMINATING WATER-COOLED REACTOR CIRCUITS | 1999 |
|
RU2169957C2 |
METHOD FOR PROTECTING POWER EQUIPMENT AGAINST CORROSION | 2003 |
|
RU2271410C2 |
METHOD OF PROTECTING STEEL AGAINST CORROSION | 1996 |
|
RU2124579C1 |
CORROSION-RESISTANT STEEL | 1993 |
|
RU2039120C1 |
COMPLEX RUST AND FOULING PROTECTION (Variants) | 1995 |
|
RU2113544C1 |
Authors
Dates
1998-08-27—Published
1995-10-18—Filed