FIELD: manufacture of sealing friction units. SUBSTANCE: method comprises treating rubbers with solution of reactive agents in organic solvent and subsequently treating them at vulcanization temperature for 40-60 minutes. Reactive agents include 2-mercaptobenzthiazole and sulfur in combination with ultradispersive powder of solid lubricating materials at concentration of 4-5, 1-2 and 8- 10 wt parts respectively, and treatment of rubber is carried out for 5-7 hours. EFFECT: lower friction coefficient with respect to metals and higher wear resistance of rubbers. 2 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS OF SURFACE MODIFICATION OF RUBBERS | 2005 |
|
RU2307842C2 |
METHOD OF SURFACE MODIFICATION OF RUBBERS | 1997 |
|
RU2129129C1 |
METHOD OF SURFACE MODIFICATION OF RESINS | 1997 |
|
RU2129128C1 |
METHOD FOR SURFACE MODIFICATION OF RUBBERS | 2000 |
|
RU2202566C2 |
METHOD OF SUPERFICIALLY MODIFYING RUBBERS | 1999 |
|
RU2169159C2 |
COMPOSITE MATERIALS FOR COMPATIBILITY OF COMMINUTED RUBBER GRANULATED MATERIALS WITH INGRADIENTS OF RUBBER BLENDS | 2001 |
|
RU2216555C2 |
METHOD OF SURFACE MODIFICATION OF RUBBER | 1986 |
|
SU1445159A1 |
FLUORINE RUBBER-BASED COATING FORMATION METHOD | 2002 |
|
RU2232780C2 |
VULCANIZATE MODIFICATION METHOD | 2002 |
|
RU2230077C2 |
CURABLE RUBBER COMPOUND | 2002 |
|
RU2236423C1 |