FIELD: rubber industry. SUBSTANCE: invention can be used in manufacture of mechanical-rubber products. Cured rubber based on carbochain rubbers is treated for 4-24 h with solution of reactive substance, in particular 2-mercaptobenzothiazole (1-2%) with sulfur (1-2%) in combination with phenol-formaldehyde resin with molecular weight 1000-2000 (8- 10%) and urotropin (0.5-1.0%), in organic solvent, which is further removed by drying. Material is then thermally treated at vulcanization temperature for 40-60 min. Products can be operated in corrosive media. EFFECT: increased oil resistance. 2 tbl, 2 ex
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF SURFACE MODIFICATION OF RUBBERS | 1997 |
|
RU2129129C1 |
| METHOD OF SURFACE MODIFICATION OF RUBBERS | 1997 |
|
RU2129130C1 |
| METHOD OF SURFACE MODIFICATION OF RESINS | 1997 |
|
RU2129128C1 |
| METHOD FOR SURFACE MODIFICATION OF RUBBERS | 2000 |
|
RU2202566C2 |
| PROCESS OF SURFACE MODIFICATION OF RUBBERS | 2005 |
|
RU2307842C2 |
| ADHESIVE SUBLAYER FOR ATTACHING RUBBER TO METAL | 2023 |
|
RU2816353C1 |
| ADHESIVE SUBLAYER FOR ATTACHING RUBBERS TO METAL | 2020 |
|
RU2774179C1 |
| FLUORINE RUBBER-BASED COATING FORMATION METHOD | 2002 |
|
RU2232780C2 |
| ADHESIVE COMPOSITION | 2009 |
|
RU2394865C1 |
| WATER-SWELLABLE ELASTOMERIC COMPOSITION | 2020 |
|
RU2744282C1 |
Authors
Dates
2001-06-20—Published
1999-04-06—Filed