FIELD: manufacture of building materials. SUBSTANCE: mixed are: rubber (chloroprene rubber, ethylene-propylene rubber, chlorinated rubber, or polybutadiene), bitumen, antioxidant, modifying additive (salicylic acid), filler, and, additionally, curing agent and synthetic resin. Prior to be mixed with bitumen, rubber is dispersed in organic solvent with antioxidant, mixture is then stirred for 15-20 min, other components are added, and stirring is continued for further 30-60 min. All operation are carried out at 20 to 60 C. Amounts of all components are specified. EFFECT: improved waterproofing properties. 5 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF BITUMINOUS-RUBBER CEMENT | 2004 |
|
RU2263692C1 |
COMPOSITION OF POLYMER-BITUMEN BINDER FOR ASPHALT-CONCRETE PAVEMENT | 2020 |
|
RU2734711C1 |
METHOD OF PREPARING RUBBER-BITUMEN MASTIC | 2000 |
|
RU2165905C1 |
MATERIAL FOR SEALING BUILDING STRUCTURES | 1998 |
|
RU2139905C1 |
COLD MASTIC FOR HYDRAULIC INSULATION AND SEALING WORKS | 2005 |
|
RU2278882C1 |
HYDRAULIC INSULATING COMPOSITION (VARIANTS) | 2004 |
|
RU2278133C2 |
COLD MASTIC FOR HYDRAULIC INSULATION (VERSIONS) | 2004 |
|
RU2280055C2 |
COLD MASTIC FOR HYDROINSULATION AND ANTICORROSION PROTECTION | 1999 |
|
RU2159786C1 |
COMPOSITION FOR MANUFACTURE OF ROLL HYDROINSULATING MATERIALS | 1992 |
|
RU2011664C1 |
COMPOSITION FOR PROTECTIVE COATING | 1999 |
|
RU2168530C1 |
Authors
Dates
1999-10-20—Published
1998-01-22—Filed