FIELD: chemical industry. SUBSTANCE: method comprises heating magnesium alloys to 280-360 C, stepwise deformation with total degree of 88-93% in several passes from one heating operation followed continuously one after another at rate of 2•10-1-6•10-2s-1 and cooling in the air. EFFECT: formation of finely dispersed structure during deformation process. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
TITANIUM-BASED ALLOY AND METHOD OF THERMAL TREATMENT OF LARGE-SIZE SEMIPRODUCTS FROM SAID ALLOY | 2000 |
|
RU2169782C1 |
TITANIUM-BASED ALLOY AND METHOD OF THERMAL TREATMENT OF LARGE-SIZE SEMIPRODUCTS FROM SAID ALLOY | 2000 |
|
RU2169204C1 |
TITANIUM-BASED ALLOY | 1999 |
|
RU2150528C1 |
METHOD FOR MAKING FORGINGS BY HOT EXTRUSION IN EXTRUDING PRESS HAVING MOVABLE CONTAINER | 2004 |
|
RU2259897C1 |
METHOD OF ROLLING BARS FROM PSEUDO β- TITANIUM ALLOYS | 2000 |
|
RU2178014C1 |
METHOD FOR HOT FORMING OF HOLLOW PRODUCTS | 2001 |
|
RU2191654C1 |
METHOD OF TREATING INGOTS OF HIGHLY REACTIVE METALS AND ALLOYS | 1994 |
|
RU2082817C1 |
METHOD FOR MAKING THIN SHEETS OF STRENGTH AND HIGH-STRENGTH ALLOYS | 2000 |
|
RU2179899C1 |
METHOD OF WORKING SEMIFINISHED PRODUCT SURFACES | 2000 |
|
RU2174461C1 |
METHOD OF PROTECTION OF SLAB SURFACES | 1998 |
|
RU2145982C1 |
Authors
Dates
2000-04-27—Published
1998-11-03—Filed