FIELD: soldering technology. SUBSTANCE: flux contains, wt.%: zinc chloride, 25-50; sodium chloride, 0.5-5; potassium chloride, 0.1-1; hydroxylamine hydrochloride, 0.1-0.4; and water, the balance. Flux ensures quality tinning and soldering of radiator cooling tubes on automated lines. EFFECT: eliminated toxicity and corrosive damages. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
FLUX FOR SOLDERING AND TINNING WITH USE OF EASY-TO-MELT SOLDER | 2000 |
|
RU2208505C2 |
FLUX FOR LOW-TEMPERATURE SOLDERING | 2004 |
|
RU2243074C1 |
CHLORIDE FLUX FOR SOLDERING | 2015 |
|
RU2599063C1 |
SOLDER FOR LOW-TEMPERATURE SOLDERING | 2002 |
|
RU2219030C1 |
METHOD OF MAKING TIN-BASED SOLDER | 2013 |
|
RU2541249C2 |
FLUX FOR LOW-TEMPERATURE SOLDERING | 2005 |
|
RU2285600C1 |
FLUX FOR SOLDERING WITH LOW-TEMPERATURE SOLDERS | 0 |
|
SU1342650A1 |
FLUX FOR LOW-TEMPERATURE SOLDERING | 2010 |
|
RU2463145C2 |
SOLDERING PASTE FOR TINNING AND SOLDERING ARTICLES OF RADIOELECTRONIC EQUIPMENT | 0 |
|
SU1532249A1 |
FLUX FOR LOW-TEMPERATURE SOLDERING | 2010 |
|
RU2463144C2 |
Authors
Dates
2000-05-20—Published
1998-08-07—Filed