FIELD: glassmaking. SUBSTANCE: float glass is manufactured by shortening length of the side spread area of glass melt flow in the drain point owing to increased width of chute and preserved the same width of manufactured tape. Ratio of the latter value to width of chute varies from 1.0 to 2.5. EFFECT: improved quality of manufactured heat-absorbing decorative glass. 1 dwg, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING GLASS STRIP OF MORE EQUILIBRIUM THICKNESS | 1998 |
|
RU2147296C1 |
METHOD OF PRODUCTION OF FLOAT-GLASS | 2001 |
|
RU2203229C2 |
METHOD OF CRYSTAL-SHEET GLASS PRODUCTION | 2000 |
|
RU2187472C2 |
METHOD OF PRODUCTION OF SHEET GLASS OF GREATER THAN EQUILIBRIUM THICKNESS | 2000 |
|
RU2181345C2 |
METHOD OF PRODUCTION OF CRYSTAL-SHEET GLASS | 2000 |
|
RU2186741C2 |
METHOD OF PRODUCTION OF SHEET GLASS OF INCREASED THICKNESS | 2005 |
|
RU2299182C1 |
METHOD OF PREPARING DECORATIVE GLASS | 2000 |
|
RU2174497C1 |
POLISHED SHEET GLASS MANUFACTURE PROCESS | 2000 |
|
RU2183203C2 |
METHOD OF PRODUCTION OF FLOAT GLASS | 2001 |
|
RU2193536C1 |
DEVICE FOR DELIVERY OF PROPORTIONED AMOUNTS OF DISPERSED MATERIAL TO GLASS BAND | 1998 |
|
RU2147015C1 |
Authors
Dates
2000-05-27—Published
1998-05-13—Filed