FIELD: technology of extraction of platinum and noble metals from various raw materials. SUBSTANCE: starting raw material is kept in inert gas atmosphere at 650 to 1000 C for 5 to 200 min. Then it is cooled in inert atmosphere and is subjected to hydraulic chlorination with hydrochloric acid and chlorine in presence of nitrate ion in the amount of 0.01 to 3.0% of volume of solution. In case raw material contains highly volatile or sulfur-containing compounds, oxidizing roasting shall be performed before keeping the material in inert atmosphere. EFFECT: facilitated process of extraction of noble components. 4 cl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
PRECIOUS METAL RECOVERY METHOD | 2002 |
|
RU2235140C2 |
METHOD OF RECOVERING PRECIOUS METALS FROM ORE PROCESSING PRODUCTS | 2016 |
|
RU2632740C1 |
METHOD OF RECOVERING PLATINUM METALS FROM PLATINUM-CONTAINING CONCENTRATES | 2000 |
|
RU2169200C1 |
METHOD OF RECOVERING AND SEPARATING PLATINUM-GROUP METALS | 2002 |
|
RU2200132C1 |
METHOD FOR PROCESSING CONCENTRATE OF PRECIOUS METALS | 1995 |
|
RU2094499C1 |
METHOD FOR PROCESSING PRODUCTS CONTAINED RUTHENIUM AND IRIDIUM | 1996 |
|
RU2104320C1 |
METHOD OF RECOVERY AND SEPARATION OF PLATINUM GROUP METALS | 2000 |
|
RU2161130C1 |
METHOD OF RECOVERY OF NOBLE METALS FROM PRODUCTS CONTAINING SILVER CHLORIDE, METALS OF PLATINUM GROUP AND GOLD | 1999 |
|
RU2164255C2 |
METHOD FOR PURIFICATION OF PLATINUM-PALLADIUM CHLORIDE SOLUTIONS FROM GOLD, SELENIUM, TELLURIUM, AND IMPURITIES OF BASE METALS | 2021 |
|
RU2787321C2 |
PLATINUM-CONTAINING CONCENTRATE PROCESSING METHOD | 2000 |
|
RU2169780C1 |
Authors
Dates
2000-08-20—Published
1999-01-13—Filed