FIELD: medicine. SUBSTANCE: method involves applying mechanical cleaning and polishing in electrolyte. Solution containing sulfuric acid, ethylene glycol and organic admixture taken in known quantitative proportions is used as electrolyte. The time required for keeping the prostheses in the solution is equal to 5 min under current density of 2-5 A/dm2, temperature of 30-45 C. Hydroxycarbonic acid of aliphatic row like citric acid is applied as the organic admixture. EFFECT: high quality of polishing; accelerated treatment method. 2 cl, 1 tbl
Authors
Dates
2000-11-27—Published
2000-04-03—Filed