FIELD: manufacture of nonwoven sorption-filtering materials. SUBSTANCE: nonwoven material has two layers fixed together by needle stitching. One layer is made from modified capron fiber megalon and other layer is made from mixture of anion-exchange fiber based on grafted copolymer of polycaproamide and polydiethylamine ethylacrylate and cation-exchange fiber based on phosphorylatedgrafted copolymer of polycaproamide and polygilicidylmethacrylate, with content of the latter in mixture being 30-70 wt.%. Weight ratio of layers is (0.2-0.4):1. EFFECT: increased efficiency and improved protective properties as to aerosol salts. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
NONWOVEN MATERIAL | 2002 |
|
RU2205255C1 |
NONWOVEN MATERIAL | 2000 |
|
RU2190049C2 |
NONWOVEN MATERIAL | 2002 |
|
RU2205256C1 |
NONWOVEN PROTECTIVE MATERIAL | 2003 |
|
RU2239676C2 |
FILTERING NONWOVEN MATERIAL | 2000 |
|
RU2166016C1 |
FILTERING NONWOVEN MATERIAL | 2000 |
|
RU2161217C1 |
NONWOVEN MATERIAL MANUFACTURE METHOD | 1995 |
|
RU2088710C1 |
NONWOVEN MATERIAL | 1995 |
|
RU2088711C1 |
NONWOVEN MATERIAL-MAKING METHOD | 1993 |
|
RU2077625C1 |
FABRIC | 0 |
|
SU1682431A1 |
Authors
Dates
2002-10-10—Published
2001-10-08—Filed