FIELD: polymer materials. SUBSTANCE: invention is dealing with adhesion polymer compositions containing 15-25% natural and/or synthetic rubber with average molecular weight above 20000 and high degree of crystallinity. Method involves mixing of crude solid polymer and, if necessary, auxiliary substances and various additives with organic solvent or solvent mixture. Further, mixture is vigorously stirred in turbulent mode at needed Reynolds criterion and during a period of time long enough to destroy polymer and completely dissolve it thereby forming homogenous mass. Auxiliary substances and various additives can possibly be added during stirring. EFFECT: simplified technology, reduced process time, reduced power and materials consumption, and improved environmental condition. 2 cl, 1 tbl, 8 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING RUBBER GLUE | 1991 |
|
RU2014338C1 |
ADHESIVE COMPOSITION | 2011 |
|
RU2463327C1 |
GLUE | 0 |
|
SU732344A1 |
METHOD OF PRODUCTION OF RUBBER MIX ON BASE OF CHLOROPRENE RUBBER FOR ADHESIVE COMPOSITION | 2005 |
|
RU2279448C1 |
METHOD OF PRODUCING 1-CALKYL- AND 1-PHENYL-5-IODOTETRAZOLES | 2011 |
|
RU2470925C1 |
METHOD AND DEVICE FOR COOLING OF WORKING MEDIUM AND METHOD FOR GENERATION OF MICROWAVE RADIATION | 2001 |
|
RU2182689C1 |
METHOD OF PREPARING BASE POLYMER SOLUTION FOR PRODUCING HALOBUTYL RUBBER | 2012 |
|
RU2484106C1 |
METHOD OF PRODUCING ANTI-TURBULENT ADDITIVE FOR ORGANIC MEDIA FOR REDUCING HYDRODYNAMIC RESISTANCE DURING TRANSPORTATION THEREOF | 2014 |
|
RU2576004C2 |
POLYFUNCTIONAL LIGHT-WEIGHT RUBBERISED PROTECTIVE MATERIAL AND PRODUCTION METHOD THEREOF | 2009 |
|
RU2429974C2 |
ADHESIVE COMPOSITION | 2010 |
|
RU2435815C1 |
Authors
Dates
2003-07-27—Published
2001-06-14—Filed