FIELD: manufacture of building materials. SUBSTANCE: composition contains, wt parts: organic sulfonate liquid glass 1.6-3.0, calcium chloride, and water 30.2-31.2, weight ratio of liquid glass to calcium chloride being 1: (0.25-0.3). Components are mixed in the form of their aqueous solutions prepared at following ratios: organic sulfonate 1:(16-20), liquid glass 1: (4-7), and calcium chloride 1: (6-11). First, liquid glass and calcium chloride solutions are mixed and then organic sulfonate solution is added. EFFECT: decreased shrinkage of cured concrete mix in the first day after curing. 2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
MOULDING MIX FOR PREPARATION OF FOAM CONCRETE | 2022 |
|
RU2802407C2 |
METHOD OF MANUFACTURING FOAMED CONCRETE AND CONCRETE MANUFACTURED BY THIS METHOD | 2001 |
|
RU2239615C2 |
FOAMED CONCRETE | 2008 |
|
RU2406710C2 |
METHOD OF PREPARING CELLULAR CONCRETE MIX | 1998 |
|
RU2139268C1 |
AUTOCLAVE FOAMED CONCRETE MIXTURE | 2009 |
|
RU2394795C1 |
RAW MATERIAL MIXTURE FOR AUTOCLAVE FOAM CONCRETE | 2013 |
|
RU2542011C1 |
MIXTURE FOR MAKING FOAM CONCRETE | 2015 |
|
RU2591996C1 |
METHOD OF PREPARATION OF DRY FINE FROTHING AGENT AND METHOD OF PREPARATION OF DRY RAW MIX FOR FOAM CONCRETE WITH USE OF THIS FROTHING AGENT | 2007 |
|
RU2342347C2 |
FOAM CONCRETE MIX AND METHOD OF PREPARATION OF SUCH MIX | 2005 |
|
RU2292322C1 |
METHOD OF PRODUCING ARTICLES FROM FOAM CONCRETE NOT AUTOCLAVED | 2011 |
|
RU2478469C1 |
Authors
Dates
2003-09-20—Published
2002-03-12—Filed