FIELD: non-ferrous metallurgy, possibly production of aluminum in cells with self-firing anode and lateral supply of electric current. SUBSTANCE: method comprises steps of interrupting charging of anode mass into anode body when 45 - 90 days are left until cutting off electric power supply; de-energizing cell when height of fired part of anode reaches 60 - 80 cm; realizing electric current supply to anode by means of two lower rows of pins. EFFECT: lowered cost of recovery of waste anode at reconstruction of cell. 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD TO FORM SELF-BAKING ANODE OF TOP-WORKED ALUMINIUM ELECTROLYTIC CELL | 2013 |
|
RU2529319C1 |
ELECTROLYZER WITH SIDE CURRENT SUPPLY TO ANODES FOR PRODUCTION OF ALUMINUM | 2000 |
|
RU2186881C1 |
METHOD FOR FORMING SELF-CALCINATING ANODE OF ALUMINIUM ELECTROLYSER WITH UPPER CURRENT LEAD | 2015 |
|
RU2606365C1 |
METHOD FOR MAKING SELF-FIRING ANODE | 2001 |
|
RU2215065C2 |
NON-CONSUMABLE ANODE DEVICE OF ALUMINIUM CELLS | 2000 |
|
RU2184179C2 |
METHOD FOR CURRENT LEAD TO ALUMINIUM ELECTROLYSER DEVICE WITH SELF-BURNING ANODE AND UPPER CURRENT LEAD | 2015 |
|
RU2613839C2 |
METHOD OF FORMING A SECONDARY ANODE OF AN ALUMINUM ELECTROLYSIS CELL WITH A SELF-BAKING ANODE | 2019 |
|
RU2698121C1 |
METHOD FOR SHAPING SELF-FIRING ANODE OF ALUMINUM CELL WITH UPPER ELECTRIC CURRENT SUPPLY LEAD | 2004 |
|
RU2255146C1 |
METHOD OF ROASTING AND STARTING ELECTROLYZER FOR OBTAINING ALUMINIUM | 0 |
|
SU1740499A1 |
METHOD OF MOUNTING THE ANODE ASSEMBLY OF ALUMINIUM ELECTROLYZER | 0 |
|
SU1407997A1 |