FIELD: shaped charges. SUBSTANCE: a mix powders including tungsten, metal binder and grease is prepared. Mixing of powders is conducted with an additional milling and activation of the surface of particles in a ball mill with steel balls exceeding the mass of the mix of powders approximately by 30 and more times during at least 4 hours. Compaction is performed at a unit pressure exceeding 500 Mpa/sq.cm. EFFECT: enhanced density of the shaped-charge facing with the compactness capability of the composite compound remaining unchanged. 3 cl, 1 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
SHAPED CHARGE FOR PERFORATOR AND SHAPED CHARGE PRODUCTION METHOD | 2005 |
|
RU2315857C2 |
SHAPED CHARGE WITH BIMETALLIC FACING AND METHOD FOR ITS MANUFACTURE | 1999 |
|
RU2151362C1 |
COMPOSITION OF MIXTURE FOR MAKING OUTER LINING OF SHAPED CHARGES | 2022 |
|
RU2817239C1 |
METHOD OF ENCASEMENT PRODUCTION FOR CUMULATIVE CHARGE FROM COMPOSITE PSEUDOALLOY Mo-Cu | 2006 |
|
RU2337308C2 |
CUMULATIVE CHARGE COATING | 2006 |
|
RU2337307C2 |
MANUFACTURING METHOD OF HIGH-TEMPERATURE ANTIFRICTION MATERIAL | 2013 |
|
RU2542039C1 |
LINING OF SHAPED CHARGE | 2002 |
|
RU2258195C1 |
METHOD OF MAKING SHAPED FACING OF DRILLING MACHINE CHARGE | 0 |
|
SU1789320A1 |
METHOD FOR MANUFACTURING SHAPED CHARGE CLADDING | 2021 |
|
RU2771470C1 |
SHAPED CHARGE, FACING OF SHAPED CHARGE (MODIFICATIONS)AND METHOD FOR ITS PRODUCTION | 2001 |
|
RU2253831C2 |
Authors
Dates
2004-06-10—Published
2002-08-22—Filed