FIELD: non-iron metallurgy, in particular manufacturing of addition alloy, modifier, solder alloy and past.
SUBSTANCE: Claimed method includes preparation of batch by mixing of copper particles and red phosphorous powder, heating, conditioning and cooling, while batch in reactor is continuously mixed. Heating, conditioning and cooling are carried out in moving closed reactor in the presence of grinding bodies. Temperature of heating and conditioning is lower than eutectic temperature in copper-phosphorous system (namely of 7140C).
EFFECT: reduced cost for producing of copper phosphide and environmental acceptability.
1 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF COPPER-PHOSPHORUS ALLOYING COMPOSITION PRODUCTION | 2000 |
|
RU2198950C2 |
METHOD OF PRODUCING COPPER-PHOSPHORUS ALLOYING ADDITIVE | 0 |
|
SU1788059A1 |
METHOD OF MAKING SOLDER | 2015 |
|
RU2598734C1 |
METHOD FOR PRODUCTION OF ALLOYS OF METALS WITH PHOSPHOROUS | 1993 |
|
RU2073735C1 |
ELECTRIC CONTACT WIRE MANUFACTURING METHOD AND ELECTRIC CONTACT WIRE | 2013 |
|
RU2540944C1 |
METHOD OF PREPARING COPPER-PHOSPHORUS MASTER ALLOY | 2000 |
|
RU2171310C1 |
METHOD OF PREPARING COPPER PHOSPHIDES | 1996 |
|
RU2108965C1 |
METHOD FOR PRODUCING MOLYBDENUM-COPPER COMPOSITION MATERIAL | 2005 |
|
RU2292988C1 |
METHOD OF PRODUCING WEAR-RESISTANT WHITE IRON | 2009 |
|
RU2412780C1 |
METHOD OF PRODUCING CRYSTALLINE POWDER OF CHROMIUM-NICKEL SPINEL | 2019 |
|
RU2726082C1 |
Authors
Dates
2004-11-27—Published
2003-03-20—Filed