FIELD: restoration of banded rollers of coilers of hot rolling mills.
SUBSTANCE: method comprises steps of preheating roller until temperature 250 -300 C; multi-layer surfacing by means of steel electrode at rate 20 -30 m/h at electric current density 20 - 25 A/sq. m; realizing heat treatment of surfaced band of roller due to heating roller until temperature 400- 450 C for time interval 5 - 7 hours.
EFFECT: increased rigidity and wear resistance of banded roller.
2 cl, 2 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
BANDED ROLLER RESTORING METHOD | 2005 |
|
RU2291041C1 |
ROLLER RESTORING METHOD | 2003 |
|
RU2243076C1 |
METHOD OF ROLL CHOCKS HYDRAULIC CYLINDER PLUNGER RESTORATION WITH FUSING | 2006 |
|
RU2327555C1 |
SHROUDING RING OF ROLLER AND PROCESS OF ITS MANUFACTURE | 1997 |
|
RU2124962C1 |
METHOD FOR RESTORING ROLLING ROLLS | 2003 |
|
RU2245771C2 |
METHOD FOR ROLLER RESTORING | 2005 |
|
RU2291040C1 |
METHOD OF REPAIR OF SHROUDED ROLLERS OF SECONDARY COOLING ZONE OF CONTINUOUS CASTING MACHINES | 1993 |
|
RU2113962C1 |
METHOD FOR RESTORING ROLLING ROLLS | 2001 |
|
RU2202422C2 |
PROCESS FOR RESTORING ROLLING ROLLS | 2003 |
|
RU2237563C1 |
METHOD FOR RESTORING CAST IRON ROLLING ROLLS WITH DAMAGED JOURNALS | 2004 |
|
RU2281846C1 |
Authors
Dates
2004-12-20—Published
2003-05-07—Filed