FIELD: inorganic compounds technologies.
SUBSTANCE: invention relates to technology of titanium-calcium mineral raw material, in particular to acid decomposition of sphene concentrate, and can be used to produce titanium dioxide and products based thereof. Prior to be treated with acid, concentrate is subjected to mechanical activation with energy supply intensity 10 kJ/s per 1 kg concentrate within 5 to 30 min. Mechanical activation in carbon dioxide medium is also possible at CO2 consumption 0.2-0,8 mole/mole CaO. For acid treatment of concentrate, 15-20% nitric acid is used at ambient temperature and atmospheric pressure, wherein additional titanium is transferred into solution. Resulting reaction mass is filtered to separate silica residue.
EFFECT: increased feasibility of process due to reduced acid treatment temperature and allowed atmospheric pressure.
2 cl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING BADDELEYITE CONCENTRATE | 2012 |
|
RU2508412C1 |
METHOD FOR DECOMPOSITION OF TITANIUM-CALCIUM RAW | 2002 |
|
RU2219130C2 |
PROCESS OF DISINTEGRATION OF TITANIUM-CALCIUM BASIC MATERIAL | 2001 |
|
RU2196736C1 |
SPHENE CONCENTRATE PROCESSING METHOD | 2005 |
|
RU2293131C1 |
METHOD FOR PROCESSING SPHENE CONCENTRATE | 2006 |
|
RU2323881C1 |
SPHENE CONCENTRATE PROCESSING METHOD | 2003 |
|
RU2235685C1 |
METHOD OF OPENING PEROVSKITE CONCENTRATES | 2013 |
|
RU2525025C1 |
METHOD FOR OPENING LOPARITE CONCENTRATES | 2012 |
|
RU2506333C1 |
PROCESSING METHOD OF ARIZONITE AND ILMENITE CONCENTRATES | 2012 |
|
RU2490346C1 |
METHOD OF SPHENE CONCENTRATE PROCESSING | 1996 |
|
RU2096331C1 |
Authors
Dates
2005-08-10—Published
2003-11-19—Filed