FIELD: leather industry.
SUBSTANCE: preparation of composition is conducted on vertical-type bead mill. Induline, kerosene, and diesel fuel are consecutively charged into mill before stirring mechanism is energized, after which apparatus and contents thereof are slowly heated. Stirring is then stopped for 1 h while slow heating of mill contents is continued. When specified time expires, carboxylic acid or acid mixture, white spirit, fat additive, and aluminum oxide or hydroxide are added. Mechanic stirring is then switched on and contents of the bead mill are ground and the process is carried out at spontaneously fixed temperature caused by heat effects of the processes and natural cooling. When temperature is lowered to 85-120°C, desired product is discharged.
EFFECT: simplified process and increased product discharge degree.
1 tbl, 19 ex