FIELD: metallurgy, possibly steel melting, particularly steel killing in ladle, in steel melting aggregate and in aggregate for out-of-furnace treatment of steel.
SUBSTANCE: process comprises steps of adding aluminum to melt steel; using aluminum in the form of ferroaluminum containing 20 - 40% of aluminum with substitution factor in relation to secondary pig aluminum 1.2 - 1.6 and with lump size 20 - 80 mm. It provides total consumption of aluminum lowered by 1.2 - 1.6 times.
EFFECT: improved assimilation of aluminum, lowered total consumption of aluminum.
4 cl, 1 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF STEEL DEOXIDATION IN LADLE | 2014 |
|
RU2562848C1 |
LOW-SILICON STEEL PRODUCTION METHOD | 2023 |
|
RU2818526C1 |
OUT-OF-FURNACE STEEL TREATMENT METHOD | 2010 |
|
RU2440421C1 |
METHOD OF PRODUCTION OF THE CARBON STEEL | 2006 |
|
RU2304622C1 |
ACTIVE DEOXIDIZER OF LIQUID AND REFRACTORY HOT AND COLD SLAGS | 2022 |
|
RU2786789C1 |
METHOD OF MAKING STEEL | 2003 |
|
RU2233339C1 |
METHOD OF LOW-CARBON STEEL DEOXIDATION | 2012 |
|
RU2514125C1 |
METHOD OF DRY STEEL PRODUCTION | 2013 |
|
RU2533263C1 |
METHOD OF OUT-OF-FURNACE TREATMENT OF STEEL IN LADLE | 2020 |
|
RU2735697C1 |
METHOD FOR THE PRODUCTION OF VANADIUM-CONTAINING STEEL (OPTIONS) | 2022 |
|
RU2786100C1 |
Authors
Dates
2006-04-27—Published
2004-07-12—Filed