FIELD: mechanical engineering and metalworking; methods of manufacture of cold strain dies.
SUBSTANCE: proposed method includes welding-on the welding material on working section of die of the following chemical composition: C, 0.5-1.5%; Si, 0.2-2.0%; Mn, 0.3-6.0%; Cr, 0.3-10%; Co, 0.3-10%; V, 0.3-2.0%; Mo, 5.0-10.0%, unavoidable admixtures; the remainder being Fe. Welded-on metal is cooled down at rate above critical rate of hardening in temperature interval of Ar1-600°C. Welded-on working part is subjected to machining for obtaining required geometry and to treatment by cold of welded-on metal. After machining and treatment by cold, welded-on metal is tempered at temperature of 480-520°C ensuring separation of dispersed carbides and intermetallic compounds without coagulation.
EFFECT: enhanced hardness of working part of die; enhanced reliability; increased productivity.
2 cl, 4 dwg, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
FLUX CORED ELECTRODE | 2007 |
|
RU2356715C2 |
DIE ALLOY | 2011 |
|
RU2479664C1 |
TOOL DIE STEEL | 2004 |
|
RU2274673C2 |
FLUX CORED WIRE | 2018 |
|
RU2682940C1 |
FLUX CORED ELECTRODE | 2007 |
|
RU2356714C2 |
PRODUCTION TILLAGE TOOL WORKING MEMBERS | 2013 |
|
RU2528687C1 |
FLUX CORED WIRE | 2020 |
|
RU2736537C1 |
DIE ALLOY | 2020 |
|
RU2727463C1 |
FLUX CORED WIRE | 2014 |
|
RU2582402C1 |
POWDER WIRE | 2011 |
|
RU2467854C1 |
Authors
Dates
2006-07-20—Published
2004-11-09—Filed