FIELD: foundry, possibly manufacture of casting molds in mass, large-scale and piece production processes.
SUBSTANCE: casting molds and cores are made from molding sands on base of organic binders, After assembling mold, liquid metal is poured into it. Simultaneously mold is blown through ventilation ducts by air heated up to temperature 300 - 700°C. Blowing is realized at rate 2 -20 l/min. Oxidation catalysts are used for neutralizing gases separated from molding sand. Oxides selected from CuO, Co3O4, MnOx where 1.7 < x < 2.0 are used as catalysts. Catalysts may be included to molding sands. When ventilation ducts are in the form of coaxial tubular members catalysts are arranged in cavity between said members.
EFFECT: highly effective neutralization of toxic gases from casting mold, elimination of gas-caused flaws in castings.
5 cl, 5 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF CAST MANUFACTURING BY HEARTH MOLDING | 2006 |
|
RU2331494C2 |
METHOD OF CASTING | 2015 |
|
RU2645824C1 |
METHOD OF DEFINING TOXIC GAS RELEASE VOLUME AND COMPOSITION | 2010 |
|
RU2455109C2 |
METHOD OF OBTAINING CASTS | 0 |
|
SU1712060A1 |
APPARATUS FOR DETECTING GAS PERMEABILITY OF MOLDING AND CORE SANDS | 2004 |
|
RU2272693C2 |
APPARATUS FOR DETERMINING SEPARATION SPEED OF TOXIC GASES OUT OF POURED CASTING MOLDS | 2003 |
|
RU2247624C2 |
DEVICE FOR PRODUCTION OF PISTON PATTERNS | 2009 |
|
RU2513672C2 |
METHOD OF CASTING OF SCREW PROPELLER FROM COPPER-BASE ALLOYS | 1996 |
|
RU2089342C1 |
GATING SYSTEM FOR CASTING OF LARGE-SIZE THIN-WALLED CASTINGS, WHICH ARE BODIES OF ROTATION FROM MAGNESIUM ALLOYS IN ATMOSPHERE OF PROTECTIVE GAS, INTO MOLDS FROM CHM | 2019 |
|
RU2738170C1 |
DEVICE TO PRODUCE PISTON CASTING | 2009 |
|
RU2418651C2 |
Authors
Dates
2007-03-27—Published
2005-06-15—Filed