FIELD: drying.
SUBSTANCE: method comprises coating the article with a jacket before supplying the heat-transfer agent, supplying heat-transfer agent inside the article, drying the article at a temperature of 60-80° C for 4-10 hours, removing the jacket, and additional drying for 2-4- hours.
EFFECT: simplified method.
1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DRYING CERAMIC PRODUCTS | 2016 |
|
RU2625579C1 |
METHOD OF DRYING LARGE-SIZED COMPLEX-SHAPED CERAMIC ARTICLES | 2023 |
|
RU2826846C1 |
METHOD OF MANUFACTURING THE LINING FOR BALL MILLS FOR THE PRODUCTION OF AQUEOUS SLURRY OF QUARTZ GLASS | 2017 |
|
RU2650308C1 |
METHOD FOR MANUFACTURING LINING OF BALL MILLS FOR OBTAINING AQUEOUS QUARTZ GLASS SLURRY | 2022 |
|
RU2798973C1 |
METHOD OF ELECTROPHORETIC MOLDING OF CERAMIC ARTICLES | 2006 |
|
RU2305668C1 |
DEVICE FOR MOULDING OF CERAMIC ITEMS FROM AQUEOUS SLIPS | 2007 |
|
RU2358861C1 |
METHOD FOR MANUFACTURING OF CORE WITH EASILY DEFORMABLE COATING | 2008 |
|
RU2382696C1 |
DEVICE FOR FORMING CERAMIC ARTICLES FROM WATER SLIPS | 2015 |
|
RU2583799C1 |
METHOD OF BEDDER-SUPPORTS MANUFACTURING FOR GLASS-CERAMIC PRODUCTS BAKEOUT | 2016 |
|
RU2634771C1 |
METHOD OF MAKING ANTENNA CAP FROM GLASS-CERAMIC LITHIUM ALUMINOSILICATE MIXTURE | 2006 |
|
RU2326094C1 |
Authors
Dates
2007-05-10—Published
2005-11-07—Filed