FIELD: powder metallurgy, namely production of carbide steels.
SUBSTANCE: method comprises steps of mixing charge containing termite mixture including 78 - 82 mass % of iron scale powder and 18 - 22 mass % of aluminum powder; at mixing adding alloy cast iron in quantity consisting of 24 - 26 mass % of termite mixture and titanium carbide in quantity consisting 18 - 20 mass % of termite mixture. Melting is realized by means of self-propagation high-temperature synthesis under layer of acidic flux with thickness 8 - 10 mm.
EFFECT: high hardness and uniform structure of carbide steel.
1 ex
Title | Year | Author | Number |
---|---|---|---|
NONDETACHABLY JOINING METHOD OF ALLOY CARBIDE STEEL AND CONSTRUCTION STEEL | 2006 |
|
RU2309817C2 |
METHOD FOR PRODUCING ALLOY FROM IRON-CONTAINING PRODUCTION PROCESS REJECTED MATERIALS | 2005 |
|
RU2295424C1 |
METHOD OF PRODUCING IRON ALLOY FROM PRODUCTION WASTE | 2004 |
|
RU2262415C1 |
METHOD OF PRODUCING DOPEDIRON ALLOY FROM INDUSTRIAL WASTES | 2004 |
|
RU2277456C1 |
METHOD OF PRODUCING DOPPED IRON ALLOY FROM PRODUCTION WASTES | 2009 |
|
RU2419655C1 |
METHOD OF PRODUCING DOPPED IRON ALLOY FROM PRODUCTION WASTES | 2009 |
|
RU2419654C1 |
METHOD OF PRODUCING DOPED IRON ALLOY FROM PRODUCTION WASTES | 2009 |
|
RU2404022C1 |
METHOD OF PRODUCING DOPED IRON ALLOY FROM PRODUCTION WASTES | 2009 |
|
RU2404023C1 |
METHOD OF PRODUCING ALLOY | 2010 |
|
RU2469816C2 |
METHOD OF MANUFACTURING PRODUCTS FROM COMPOSITE MATERIAL | 2018 |
|
RU2677556C1 |
Authors
Dates
2007-06-27—Published
2005-12-14—Filed