FIELD: metallurgy.
SUBSTANCE: either a liquid or a firm binder pitch material is to be mixed with a fraction which consists of particles and contains at least about 35% mass of coke, coal and their mixtures. These particles have such a diameter that their main part can pass through a sieve with the cell sizes ranging from 0.25 mm and up to 25 mm. After completion of an at least 50% of the mixing cycle, one can add in the mixture the carbonaceous filaments whose stretching durability starts from 10546 and reaches 1054605 kgf/cm2 with the 6-15 mcm diameter. The mixture obtained is then extruded. The non-burnt partially finished product is to be burnt, and afterwards carbonated and graphitized under the temperatures no less than 2500° C. The mixture can also additionally contain filling agent with bantam size particles and an additive - an oxide of iron or an oil coke.
EFFECT: plumbaginous products are known for their heightened durability and lowered fragility.
27 cl, 4 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MAKING CARBON ELECTRODES | 2003 |
|
RU2315133C2 |
INCOMING-FEMALE CONNECTION OF ELECTRODE | 2005 |
|
RU2369047C2 |
FACE SEAL FOR GRAPHITE ELECTRODES | 2004 |
|
RU2366118C2 |
METHOD OF OBTAINING MOULDED PRODUCT FROM CARBON MATERIAL WITH APPLICATION OF RECYCLED CARBON FIBRES | 2011 |
|
RU2547184C2 |
GRAPHITIZED FOAMED BLANK | 1999 |
|
RU2225873C2 |
CONNECTING ELEMENTS FOR ELECTRODES FROM CARBON MATERIALS AND METHOD OF THEIR PRODUCTION | 2004 |
|
RU2331162C2 |
GRAPHITE ELECTRODE | 2013 |
|
RU2623446C2 |
GRAPHITE ELECTRODE | 2011 |
|
RU2559832C2 |
COKE REINFORCED WITH CARBON FIBRE, OBTAINED ON RETARDED COKING INSTALLATION | 2004 |
|
RU2343133C2 |
METHOD FOR PRODUCING MESOPHASE PITCH (VERSIONS) | 2016 |
|
RU2708848C1 |
Authors
Dates
2008-05-20—Published
2003-08-27—Filed