FIELD: chemistry.
SUBSTANCE: in the method of processing cement concrete there is successive depositing on its surface, of a 10% solution of ortho-phosphoric acid or 10-15% solution of colourless phosphate binder and after 2-3 minutes, a 8-12% solution of an iron, or zinc or barium chloride, iron or zinc or barium nitrate, or iron or zinc sulphate.
EFFECT: increased water permeability and frost resistance of concrete, increased degree of whiteness of the processed surface.
4 ex,1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF COLOURING CEMENT CONCRETE (VERSIONS) | 2006 |
|
RU2338729C2 |
COMPOSITION FOR PROTECTION OF CONCRETE SURFACES AND METHOD FOR PROTECTION OF CONCRETE SURFACES | 2008 |
|
RU2363681C1 |
MAGNESIUM PHOSPHORIC ACID CEMENTS | 2007 |
|
RU2344101C1 |
METHOD OF MAKING THE DECORATIVE BINDING AGENT OF LOW WATER REQUIREMENT | 1992 |
|
RU2085526C1 |
COMPLEX ADDITIVE AGENT TO CONCRETE MIXTURE | 2008 |
|
RU2359933C1 |
PROTECTIVE COMPOSITION FOR CONCRETE SURFACES AND METHOD FOR PROTECTING CONCRETE SURFACES | 1995 |
|
RU2072335C1 |
MULTIPURPOSE DRY CEMENT COMPOSITION | 1999 |
|
RU2181705C2 |
COLMATING COMPOSITION (VERSIONS) | 2012 |
|
RU2518584C2 |
METHOD FOR CREATING WATER-PROOFING COATING ON CONCRETE SURFACES | 1995 |
|
RU2083773C1 |
WATERPROOF COMPOUND USED FOR CONCRETE SURFACE TREATMENT | 2007 |
|
RU2350583C1 |
Authors
Dates
2008-11-20—Published