FIELD: metallurgy.
SUBSTANCE: compact-material consists of powdered filler-core, enveloped into steel shell in kind of wire or band and containing magnesium and burned dolomite. The powdered filler-core additionally contains carbon containing material and stavrolite at a following ratio of ingredients: magnesium: carbon containing material: burned dolomite: stavrolite - 1 : 1 : (6-8) : (5-7). As carbon containing material there is used a material chosen from the group: graphite, crushed electrodes, coke, while contents of magnesia in burned dolomite maintain at 25-30%.
EFFECT: reduction of magnesium losses and its upgraded efficiency owing to reduction of oxidation of stavrolite, dehydration of burned dolomite and generation of refined covering slag.
2 cl
Title | Year | Author | Number |
---|---|---|---|
COMPACT MATERIAL FOR LADLE PROCESSING OF IRON | 2006 |
|
RU2336309C2 |
POWDER WIRE FOR OUT-OF-FURNACE TREATMENT OF CAST IRON IN LADLE | 2015 |
|
RU2614915C1 |
POWDER WIRE FOR ADDITION OF MAGNESIUM TO IRON-BASED ALLOYS | 2006 |
|
RU2317337C2 |
WIRE FOR TREATMENT OF LIQUID CAST IRON IN LADLE | 2007 |
|
RU2349646C2 |
PROCEDURE FOR STEEL MAKING IN ARC STEEL MELTING FURNACE | 2010 |
|
RU2430973C1 |
ADDITIONAL WIRE FOR ADDING OF MAGNESIUM INTO IRON-BASED MELTS | 2002 |
|
RU2234539C2 |
PROCEDURE FOR TREATMENT OF STEEL IN CASTING LADLE | 2009 |
|
RU2413006C1 |
METALLURGICAL FLUX AND METHOD OF ITS MANUFACTURING | 2013 |
|
RU2547379C1 |
FLUXED CORED WIRE FILLER FOR DESULFURISING AND MODIFICATION OF CAST IRON | 2006 |
|
RU2337972C2 |
CHARGE AND METHOD OF OBTAINING FLUX AND REFRACTORY MATERIAL FOR STEEL PRODUCTION (OPTIONS) WITH ITS USE | 2020 |
|
RU2749446C1 |
Authors
Dates
2008-11-20—Published
2006-09-18—Filed