FIELD: chemistry.
SUBSTANCE: kaolin and silicon dioxide are mixed with molar ratio SiO2:Al2O3=(3-4):1, with addition of 10-30% wt of p0owder-like faujasite with crystal size 0.5-2.0 mcm and carboxylmethylcellulose, chemical processing and moistening are carried out until homogenous mixture is obtained, formation of granules, thermal activation and hydrothermal crystallisation in alkali aluminate solution with concentration Al2O3=5-50 g/l, Na2O=70-140 g/l with ratio of granule weight to solution volume equal 1:(3-5), are carried out.
EFFECT: high phase frequency, dynamic adsorption capacity and mechanical strength, efficiency in processes of natural gas drying and sulphur-refinement.
19 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING GRANULATED FAUJASITE WITH HIGH PHASE PURITY | 2007 |
|
RU2343115C1 |
METHOD OF OBTAINING HIGH-PHASE PURITY GRANULAR NaX ZEOLITE WITHOUT BINDER | 2009 |
|
RU2404122C1 |
METHOD OF PRODUCING HIGH PHASE PURITY ZEOLITE ADSORBENT OF STRUCTURE A AND X, GRANULATED WITHOUT BINDER | 2009 |
|
RU2420457C1 |
METHOD OF PREPARING GRANULATED ZEOLITE ADSORBENT WITH HIGH PHASE-PURITY STRUCTURES A AND X | 2005 |
|
RU2283278C1 |
METHOD FOR PRODUCING SYNTHETIC GRANULAR ZEOLITE OF PHOJAZITE TYPE | 2021 |
|
RU2761823C1 |
METHOD OF PRODUCING HIGH-MODULUS FAUJASITE WITHOUT BINDING MATERIALS | 2010 |
|
RU2456238C1 |
METHOD OF PREPARING HIGH-PHASE PURITY GRANULATED FAUJASITE | 2001 |
|
RU2203224C1 |
METHOD OF PREPARING HIGH PHASE-PURITY GRANULATED A-TYPE ZEOLITE | 2005 |
|
RU2283281C1 |
METHOD OF PREPARING SYNTHETIC A-TYPE ZEOLITE | 2005 |
|
RU2283280C1 |
METHOD OF PRODUCTION OF SYNTHETIC GRANULATED FAUJASITE | 2000 |
|
RU2180319C1 |
Authors
Dates
2009-01-10—Published
2007-07-16—Filed