FIELD: chemistry.
SUBSTANCE: method involves zinc plating, nickel plating. After nickel plating heat treatment is carried out at a temperature of 210°C for a period of 60 minutes followed by activation in concentrated hydrochloric acid at a temperature of 15-30°C for 1 minute.
EFFECT: simplification in preparing the surface of articles made from aluminium or its alloys before electroplating.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MAKING ASSEMBLED ARTICLES AND METHOD OF PREPARING ASSEMBLED ARTICLES BEFORE COATING SURFACES THEREOF | 2011 |
|
RU2460162C1 |
METHOD OF APPLYING GALVANIC COATINGS ON COMPLEX-PROFILE PARTS | 2019 |
|
RU2709913C1 |
METHOD OF SURFACE PREPARATION OF STAINLESS STEEL ITEMS PRIOR TO GALVANIC COPPERPLATING | 2013 |
|
RU2549037C2 |
PROCESS OF DEPOSITION OF METAL COATS ON ARTICLES MADE OF MAGNESIUM AND ITS ALLOYS | 1999 |
|
RU2150534C1 |
METHOD OF TREATING OBJECTS OF ALUMINUM AND ITS ALLOYS (VERSIONS) | 1996 |
|
RU2096533C1 |
METHOD OF PREPARING THE SURFACE OF ZIRCONIUM OR ARTICLES BASED ON GALVANIC NICKEL PLATING | 2016 |
|
RU2649112C1 |
METHOD TO PRODUCE MOTOR CARS BRAKING SYSTEM DOUBLE LAYERED ROLLED UP SOLDERED PIPES WITH COVERS | 1991 |
|
RU1807730C |
PROCEDURE FOR PREPARING SURFACE OF WIRE OF ALUMINIUM AND ITS ALLOYS FOR ELECTRO-DEPOSIT | 2010 |
|
RU2434974C1 |
METHOD FOR APPLICATION OF NICKEL COATINGS TO ALUMINUM ALLOYS | 2017 |
|
RU2661695C1 |
METHOD OF PREPARING STEEL FOR HOT GALVANIZING | 0 |
|
SU1787169A3 |
Authors
Dates
2009-03-20—Published
2007-05-14—Filed