FIELD: chemistry.
SUBSTANCE: invention relates to hardening of refinishing surfaces of steel parts by sulphidising. Sulphidising is carried our within 1-4 hours at 550- 600°C of temperature with using a coating of the following composition, wt %: sulphur pyrites 50, coal clay 50. Before sulphidising a layer of ferrum molybdene coat is electrically precipitated.
EFFECT: enhancement of wearing capacity and reliability of surfaces of steel parts.
Title | Year | Author | Number |
---|---|---|---|
STRENGTHENING METHOD OF METALLIC SURFACES SULPHOCYANIDING | 2007 |
|
RU2355815C2 |
METHOD OF HARDENING OF METALLIC SURFACES | 2004 |
|
RU2261939C1 |
METHOD OF ELECTROLYTIC PRECIPITATION OF IRON-MOLYBDENUM DISULFIDE COATING | 2013 |
|
RU2537686C1 |
METHOD OF HARDENING ELECTRODEPOSITED IRON-CHROMIUM COATINGS BY CARBONISATION | 2013 |
|
RU2537471C2 |
METHOD OF HARDENING ELECTRODEPOSITED IRON-CHROMIUM COATINGS BY CARBONITRIDING | 2013 |
|
RU2524294C1 |
METHOD OF ELECTRODEPOSITION OF FERROMOLYBDENUM ALLOY | 2000 |
|
RU2174163C1 |
METHOD OF ELECTROLYTIC DEPOSTION OF IRON-VANADIUM-COBALT ALLOY | 2009 |
|
RU2401328C1 |
ELECTROLYTE FOR DEPOSITION OF COAT | 1999 |
|
RU2169799C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF AN IRON-TITANIUM ALLOY | 2003 |
|
RU2230139C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-VANADIUM ALLOY | 2002 |
|
RU2231578C1 |
Authors
Dates
2009-06-27—Published
2007-04-16—Filed