FIELD: process engineering.
SUBSTANCE: structural defect revealed and processed, the structure is heated to 150-200°C and processed surface is coated with a thin layer of plastic chromium-nickel alloy, as well as structure surface adjoining to aforesaid processed surface. Further on, processed surface is soldered using the same alloy used in coating, or that with strength approximating to strength of base metal depending upon defect size.
EFFECT: complete elimination of defect and producing strong repair seam.
3 cl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
CASTINGS REPAIRE METHOD, USING THE ARC WELDING | 2015 |
|
RU2630080C2 |
METAL PIPELINES REPAIR METHOD IN FIELD CONDITIONS AND INSTALLATION FOR ITS IMPLEMENTATION | 2020 |
|
RU2734312C1 |
METHOD OF WELDING OF DEFECTS IN ALUMINIUM ALLOY CASTINGS | 1997 |
|
RU2109611C1 |
METHOD OF DEFECT ATTACK ON DETAILS | 2007 |
|
RU2351449C2 |
METHOD OF ELECTRIC-ARC WELDING | 1997 |
|
RU2110378C1 |
METHOD OF WELDED CONNECTION OF PIPES WITH BOTTOM OF REACTOR | 2020 |
|
RU2740128C1 |
METHOD OF WELDING OF BASE STRUCTURES MANUFACTURED OF ALUMINIUM ALLOYS | 1996 |
|
RU2089364C1 |
METHOD FOR WELDING THICK-WALLED LARGE-SIZE PARTS | 2012 |
|
RU2606144C2 |
METHOD FOR WELDING DISPERSION-HARDENING ALLOYS WITH CORROSION-RESISTANT STEELS | 2023 |
|
RU2809102C1 |
METHOD FOR CORRECTING FLAWS OF CASTINGS | 2001 |
|
RU2204467C2 |
Authors
Dates
2009-09-27—Published
2006-12-08—Filed