FIELD: metallurgy.
SUBSTANCE: obtainment of enamel coating strip free of fish-scale flaw involves continuous pouring of steel containing, wt %: carbon 0.02-0.05, aluminium 0.05 or less, nickel 0.05-0.08, boron 0.001-0.003; slab heating, hot rolling in a mill, coiling of semi-finished hot-rolled stock of 1.8-2.0 mm thickness into a roll. Slab of the temperature of 560°C or higher is placed in continuous furnace and heated at 1240-1280°C for 210-240 minutes, and coiling of semi-finished hot-rolled stock is performed at 730-760°C.
EFFECT: improved consumer characteristics.
1 ex, 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD FOR PRODUCTION OF COLD ROLLED STRIPS FOR ENAMELLING | 2008 | 
 | RU2392072C1 | 
| METHOD FOR PRODUCING OF SEMI-FINISHED HOT-ROLLED STOCK FOR MANUFACTURE OF ENAMELED ROLLED PRODUCTS | 2005 | 
 | RU2305137C2 | 
| PROCEDURE FOR PRODUCTION OF LOW CARBON COLD ROLLED STEEL FOR PRESS FORMING AND SUCCESSIVE ENAMELLING | 2010 | 
 | RU2424328C1 | 
| METHOD OF COLD-ROLLED SHEET PRODUCTS MANUFACTURING FOR ENAMELING | 2008 | 
 | RU2379361C1 | 
| PROCEDURE FOR PRODUCTION OF EXTRA LOW CARBON COLD ROLLED STEEL FOR DEEP DRAWING AND SUCCESSIVE SINGLE-LAYER ENAMELLING | 2014 | 
 | RU2547976C1 | 
| METHOD OF MANUFACTURING STRIPS FROM COLD-ROLLED SHEETS FROM LOW-CARBON TYPE-OB STEEL ALLOYED BY PHOSPHORUS (0,04-0,10 BY MASS) AND ALUMINUM (0,02-0,08 % BY MASS) FOR ENAMELLING | 1992 | 
 | RU2010634C1 | 
| METHOD OF PRODUCTION OF STEEL STRIP FOR ENAMELING | 1996 | 
 | RU2101368C1 | 
| METHOD FOR MAKING STEEL SHEET FOR ENAMELLING | 1999 | 
 | RU2165809C1 | 
| METHOD OF PRODUCTION OF COLD ROLLED NON-AGING STEEL FOR ENAMELLING | 1992 | 
 | RU2039839C1 | 
| COLD ROLLED STEEL SHEETS MAKING METHOD | 2004 | 
 | RU2268097C1 | 
Authors
Dates
2010-06-20—Published
2009-06-15—Filed