FIELD: chemistry.
SUBSTANCE: invention relates to chemical industry and non-ferrous metallurgy and can be used to produce aluminium sulphate in liquid form. To obtain aluminium sulphate, burnt kaolin clay is reacted with sulphuric acid taken in stoichiometric amount of 93-95%. The reaction is carried out in a reactor consisting of two parts - a lower part with diametre to height ratio of 0.4-0.5 and an upper part with diametre to height ratio of 2.3-2.5, while stirring the pulp with a propeller mixer turning at 40-80 rpm and jet steam at pressure of 1.5-3.5 atm, temperature of 110-125°C for 30-45 minutes. The melt formed is diluted with water until achieving Al2O3 concentration of 7.2%.
EFFECT: invention lowers the cost of the process and improves quality of the product.
2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF COAGULANT - LIQUID ALUMINUM SULFATE | 1999 |
|
RU2157341C1 |
PROCESS OF PRODUCING COAGULANT IN FORM OF LIQUID ALUMINUM SULFATE | 2001 |
|
RU2193011C1 |
METHOD OF PRODUCING GRANULATED ALUMINUM SULFATE | 2000 |
|
RU2181696C2 |
METHOD OF PRODUCING CLARIFIED MIXED ALUMINUM DIHYDROXOCHLORIDE COAGULANT | 2020 |
|
RU2741019C1 |
METHOD OF PRODUCTION OF ALUMINUM SULFATE | 2002 |
|
RU2214365C1 |
METHOD OF PRODUCING MIXED ALUMINIUM DIHYDROXOCHLORIDE COAGULANT AND SILICIC ACID COAGULANT | 2011 |
|
RU2458945C1 |
METHOD FOR REPROCESSING OF COPPER-CHLORIDE FUSION CAKE, WHICH IS WASTE FROM TITANIUM TETRACHLORIDE CLEANING | 2007 |
|
RU2340688C1 |
0 |
|
SU300417A1 | |
METHOD OF PRODUCING DICHLORODIAMMINEPALLADIUM FROM PALLADIUM-CONTAINING MATERIAL | 1996 |
|
RU2100277C1 |
METHOD FOR PREPARING COAGULATING AGENT | 2001 |
|
RU2215691C2 |
Authors
Dates
2010-10-27—Published
2006-06-29—Filed