FIELD: metallurgy.
SUBSTANCE: procedure consists in heating item in contact with powder of chromium oxide to 1000-1100°C, in conditioning at that temperature during 2-4 hours and in cooling in air.
EFFECT: deeper chromised layer on surface of iron, simplified and price-reduced process of chromium plating.
3 dwg, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DIFFUSION TITANISING OF CAST IRON PRODUCTS | 2012 |
|
RU2493289C1 |
METHOD OF FABRICATION OF BILLETS OF COINS | 2005 |
|
RU2383657C2 |
COMPOUND FOR DIFFUSION SATURATION OF IRON-CARBON ALLOYS | 0 |
|
SU1759954A1 |
METHOD OF HARDENING PARTS | 2005 |
|
RU2282677C1 |
METHOD OF OBTAINING DIFFUSION CHROMIUM COATING ON LOW-CARBON STEEL ARTCILES | 0 |
|
SU1560618A1 |
ROMANIT-FUVLHCH FRICTION COMPOSITE MATERIAL AND METHOD OF PRODUCTION THEREOF | 2016 |
|
RU2665651C2 |
METHOD FOR DRY CHROMIZING OF FORMING CHILLED CAST IRON ROLLS | 1996 |
|
RU2090647C1 |
METHOD OF PRODUCTION OF CAST IRON CASTING | 2013 |
|
RU2541250C1 |
CAST IRON FOR GRINDING BODIES | 2015 |
|
RU2627713C2 |
PROCESS OF MANUFACTURE OF PARTS WITH HARD ELECTROCHEMICAL CHROMIUM COAT | 2000 |
|
RU2180022C2 |
Authors
Dates
2010-12-20—Published
2009-04-21—Filed