FIELD: metallurgy.
SUBSTANCE: there are made samples by melting experimental ingot of charge containing addition alloy for titanium alloy and additional component in form of spongy titanium which forms homogenous alloy with addition alloy. Also, amount of controlled addition alloy in alloy comes to from 10 to 50 wt %. There is fabricated a sample out of an experimental ingot and there is performed X-ray control for presence of inclusions in composition of addition alloy containing refractory metals. By results of X-ray control there is carried out micro-X-ray-spectral assay of composition of revealed inclusions.
EFFECT: more upgraded control of addition alloy for titanium alloys.
1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING OF INTERMETALLIC ALLOYS BASED ON TITANIUM ALUMINIDE WITH INCREASED NIOBIUM CONTENT | 2014 |
|
RU2576288C1 |
METHOD TO PRODUCE INGOT OF PSEUDO β-TITANIUM ALLOY, CONTAINING (4,0-6,0)%Al, (4,5-6,0)% Mo, (4,5-6,0)% V, (2,0-3,6)%Cr, (0,2-0,5)% Fe, (0,1-2,0)%Zr | 2010 |
|
RU2463365C2 |
METHOD OF PRODUCTION OF INGOTS | 2005 |
|
RU2317343C2 |
PROCESS FOR MANUFACTURING TITANIUM ALLOY INGOTS | 1991 |
|
RU2031174C1 |
FURNACE FOR MELTING AND REFINING OF REACTION METALS AND ALLOYS | 2009 |
|
RU2426804C1 |
METHOD FOR PRODUCING OF INGOTS | 2003 |
|
RU2263721C2 |
METHOD OF AUTOCRUCIBLE MELTING OF METALS AND SLAG LINING FURNACE FOR REALIZATION OF THIS METHOD | 2003 |
|
RU2246547C1 |
MELTING METHOD OF REACTIVE METALS AND ALLOYS ON ITS BASIS | 2012 |
|
RU2630138C2 |
VACUUM ELECTRIC-ARC SCULL FURNACE | 2005 |
|
RU2288287C2 |
SECONDARY TITANIUM ALLOY AND PROCEDURE FOR ITS FABRICATION | 2010 |
|
RU2425164C1 |
Authors
Dates
2011-07-27—Published
2009-10-12—Filed