FIELD: chemistry.
SUBSTANCE: porous aluminium oxide layer with thickness of 20-30 mcm is formed via anodic treatment in aqueous solutions of acids of aluminium or alloys thereof, saturated with aqueous solution of a silver salt with concentration of 10-4-10-2 M/l, dried, treated with aqueous solution of potassium or sodium bromide, dried, treated with ultraviolet radiation and then with hydroquinone developer in order to form in the aluminium oxide pores silver particles whose dimensions do not exceed 20-70 nm and which do not exceed the diameter of aluminium oxide pores. Concentration of potassium bromide is equal to 10-2-10-1 M/l.
EFFECT: invention enables to produce a nanocomposite coating on porous aluminium oxide.
2 cl, 2 dwg, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR FORMING HYBRID COATING ON ALUMINUM | 2023 |
|
RU2796602C1 |
TECHNIQUE OF OXIDE COATING ON ALUMINIUM AND ITS ALLOYS | 2007 |
|
RU2353717C1 |
METHOD FOR PRODUCING CATALYTICALLY ACTIVE COMPOSITE MATERIAL | 2017 |
|
RU2641290C1 |
METHOD OF ANTICORROSION PROCESSING OF ALUMINIUM ALLOYS | 2013 |
|
RU2528285C1 |
METHOD FOR MANUFACTURE OF MEMBRANES | 0 |
|
SU1695970A1 |
METHOD OF FORMING POROUS OXIDE ON TITANIUM-ALUMINIUM ALLOY | 2011 |
|
RU2509181C2 |
METHOD OF DIAPHRAGM MANUFACTURE | 0 |
|
SU1775146A1 |
ELASTIC ALUMINA NANO-MEMBRANE OBTAINING METHOD | 2017 |
|
RU2678055C2 |
METHOD FOR FORMATION OF CRYSTAL NANO-POROUS OXIDE ON TITANIUM-ALUMINIUM ALLOY | 2015 |
|
RU2601904C2 |
PRINTED-CIRCUIT BOARD MANUFACTURING PROCESS | 1991 |
|
RU2022496C1 |
Authors
Dates
2011-08-10—Published
2009-05-18—Filed