FIELD: chemistry.
SUBSTANCE: invention relates to a method of producing a hydrotreatment catalyst. Described is a method of producing a hydrotreatment catalyst which involves the following steps: a) at least one step for saturating a dried and/or annealed catalyst precursor containing at least one group VIII element and/or at least one group VIB element and an amorphous support using an impregnating solution consisting of at least one phosphorus-containing compound dissolved in at least one polar solvent with relative permittivity higher than 20; b) a step for maturation of said saturated catalyst precursor obtained at step a); wherein said maturation step is carried out at atmospheric pressure, at temperature ranging from ambient temperature to 60°C for maturation period of 12 to 340 hours; c) a step for drying without a subsequent step for annealing said catalyst precursor obtained at step b), wherein the drying step c) is carried out in a drying oven at atmospheric or low pressure and at temperature 50-200°C. Described is use of the catalyst obtained using the described method to carry out hydrofining and hydroconversion of hydrocarbon material.
EFFECT: high catalyst activity.
14 cl, 8 tbl, 17 ex
Authors
Dates
2012-05-27—Published
2008-06-03—Filed