FIELD: process engineering.
SUBSTANCE: proposed method comprises processing initial cellulose fibrous material by liquid-phase composition containing silanol groups with molecular weight varying from 900 to 2400 and viscosity varying from 520 to 1700 cPs, and 2-7%-water solution of fire retardant. Processed material is dried to 105-125°C for 60-120 min. Then, carbonisation is performed in air at 140-170°C for 25-40 min. Carbonisation is terminated at 700°C to proceed with high-temperature processing at, at least, 2200°C.
EFFECT: high physical properties and yield.
4 cl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING CARBON FIBER MATERIAL | 2012 |
|
RU2490378C1 |
METHOD FOR OBTAINING CARBON FIBRE AND MATERIALS ON ITS BASIS | 2008 |
|
RU2384657C2 |
METHOD FOR MAKING CARBON FIBER MATERIAL | 2014 |
|
RU2577578C1 |
METHOD OF PRODUCING CARBON FIBRE AND MATERIALS BASED ON CARBON FIBRE | 2010 |
|
RU2424385C1 |
METHOD OF PRODUCING CARBON FIBER AND BASED MATERIALS | 2020 |
|
RU2741012C1 |
METHOD OF CARBON FIBROUS MATERIAL PRODUCING | 1993 |
|
RU2047674C1 |
CARBON SORPTION WOUND DRESSING FROM CARBON FIBROUS MATERIAL | 2019 |
|
RU2701141C1 |
CARBON DRESSING FOR FIRST LAYER OF NON-TRAUMATIC BANDAGE AS WOUND COATING FROM CARBON FIBROUS MATERIAL | 2019 |
|
RU2704609C1 |
APPARATUS FOR PRODUCING CARBON FIBER MATERIALS | 2015 |
|
RU2645208C2 |
METHOD OF PRODUCING CARBON FIBRE MATERIALS | 2015 |
|
RU2596752C1 |
Authors
Dates
2012-08-27—Published
2011-03-18—Filed