FIELD: metallurgy.
SUBSTANCE: briquetted charge of chemical agent of zinc oxide, which is annealed at temperature of 1100°C during 20 hours, is used; the above charge is subject to hydro thermal re-crystallisation from potassium hydroxide solution with addition of lithium ions in tight vessels from corrosion resistant material to seeding plates oriented parallel to hemihedral edges (0001) and cut from pre-grown hydrothermal crystals of zinc oxide.
EFFECT: obtaining high-quality zinc oxide crystals on a commercial scale.
1 ex
Title | Year | Author | Number |
---|---|---|---|
ZINC OXIDE CRYSTALS GROWING METHOD | 2006 |
|
RU2320787C1 |
METHOD OF ZINCITE CRYSTAL GROWING | 2001 |
|
RU2198250C1 |
METHOD OF PRODUCING OPTICAL CALCITE SINGLE CRYSTALS | 2001 |
|
RU2194806C1 |
METHOD OF PRODUCING COLORED ZINC OXIDE SINGLE CRYSTALS | 0 |
|
SU1673651A1 |
METHOD OF PRODUCING SINGLE CRYSTALS OF NEPHELINE | 0 |
|
SU1701756A1 |
METHOD FOR PRODUCTION OF ARTIFICIAL AMETHYST | 1992 |
|
RU2040596C1 |
METHOD OF GROWING ZINC OXIDE SINGLE CRYSTALS FOR LASERS | 0 |
|
SU1668495A1 |
METHOD OF PREPARING ARTIFICIAL QUARTZ CRYSTALS | 2003 |
|
RU2236489C1 |
0 |
|
SU442827A1 | |
METHOD OF PREPARING SYNTHETIC QUARTZ MONOCRYSTALS | 1996 |
|
RU2120502C1 |
Authors
Dates
2012-09-10—Published
2010-06-18—Filed