FIELD: metallurgy.
SUBSTANCE: proposed method comprises built-up steel surface forming, cooling and tempering. Note here that said surface forming is conducted during cooling after building up at (Mm+80)°C to 60°C, where Mm is martensitic transformation temperature of built-up high-speed steel. Single tempering is performed at 520-540°C and cured for 20-40 min.
EFFECT: higher hardness.
1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
PRODUCTION OF BUILT-UP CUTTING TOOL | 2013 |
|
RU2539499C1 |
METHOD FOR MANUFACTURING WELD BIMETALLIC CUTTING TOOL | 2016 |
|
RU2627837C1 |
METHOD OF MULTILAYER SURFACING WITH HIGH-HEAT STEELS OF HIGH HARDNESS IN NITROGEN-CONTAINING MEDIUM | 2019 |
|
RU2699488C1 |
POWDER WIRE | 2011 |
|
RU2467854C1 |
FLUX CORED WIRE | 2010 |
|
RU2429957C1 |
PRODUCTION OF SMALL-SIZE CUTTING TOOLS FROM HIGH-SPEED STEEL | 2014 |
|
RU2563382C1 |
METHOD FOR SURFACING WITH HARDENING BY STRAIN WAVE | 2020 |
|
RU2759278C1 |
FLUX CORED WIRE | 2020 |
|
RU2736537C1 |
FLUX CORED WIRE | 2018 |
|
RU2679374C1 |
METHOD OF THERMALLY TREATING HIGH-SPEED STEEL | 0 |
|
SU1749268A1 |
Authors
Dates
2013-05-27—Published
2012-05-22—Filed