FIELD: machine building.
SUBSTANCE: method of layer-by-layer wear-resistant building-up welding of steel bearing races of rotary supports of jib cranes in the medium of shielding gases includes the making of layers without preheating and after-welding heat treatment. The building-up welding is performed by stably austenitic welding materials in conditions excluding the quenching of the detail under the first layer. After building-up welding of the first layer and its curing the building-up welding of the second and consequent layers with chrome-manganese materials in conditions excluding the mixing and through penetration of the first layer, and also quenching of built-up detail. The first layer is made at a forward speed 2-5 m/h with stably austenitic welding materials of the type Sv-Kh15N25AM6 or welding rods EA-395/9, NIAT-5, ANZhR-1, ANZhR-2 and EA-48/N22. The second and consequent layers are made at a speed 18-25 m/h with austenitic chrome-manganese materials of the type Sv-Kh18N7G7 or welding rods TsNIIN-4.
EFFECT: excluding possibility of formation of hardening patterns in quenched steel, which result to cooling cracks under the building-up welding.
2 cl, 3 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ELECTRIC-ARC WELDING | 1997 |
|
RU2110378C1 |
METHOD OF SUBMERGED TWIN-ARC WELDING OF STEEL | 1991 |
|
RU2023556C1 |
METHOD FOR STRENGTHENING STEEL PARTS | 0 |
|
SU969757A1 |
POWDER WIRE FOR SURFACING WITH USE OF OPEN ELECTRIC ARC | 2002 |
|
RU2228829C1 |
HIGHLY PRODUCTIVE AUTOMATIC SUBMERGED ARC-CONTACT SURFACING METHOD WITH FILLER WIRE TRANSVERSE VIBRATIONS | 2015 |
|
RU2613800C2 |
METHOD FOR ELECTRIC ARC DOUBLE-LAYER WELDING-ON | 1999 |
|
RU2159171C1 |
METHOD FOR ELECTRIC-ARC WELDING OF MULTI-PASS JOINTS | 2003 |
|
RU2252116C2 |
BLEND FOR FLUX-CORED WIRE | 1993 |
|
RU2074078C1 |
SUBMERGED ARC-WELDING METHOD WITH ADDITIONAL ADDITIVE | 2020 |
|
RU2735084C1 |
METHOD OF RESTORING WEARED SURFACE OF TRAM RAIL | 2016 |
|
RU2624752C1 |
Authors
Dates
2014-10-20—Published
2013-04-19—Filed