FIELD: electricity.
SUBSTANCE: manufacturing technique of high-build wear-resistant coating in microarc oxidation mode includes installation of a part in electrolyte at a current-conducting holder coated by insulating material, generation of operating voltage between a part and electrolyte, increase of voltage till microarc discharge occurs at the surface of a part. Aqueous solution of potassium hydroxide and soluble glass is used as electrolyte at concentration of each substance of 2.5 g/l, microarc oxidation process is carried during 2.5-3.5 hours at current of I=4.5-12 A, ratio of anodic and cathodic current is 1:1 and voltage at anode is Ua=200-415 V.
EFFECT: invention allows manufacturing high-build wear-resistant coating by microarc oxidation with increased values of microhardness, reducing labour intensity and energy consumption due to optimal concentration of substances included into the electrolyte composition and optimal parameters of microarc oxidation process.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING THICK-LAYER HEAT-SHIELDING COATINGS BY MICROARC OXIDATION ON HIGH-SILICON ALUMINUM ALLOY | 2018 |
|
RU2694441C1 |
METHOD OF RECONDITIONING PARTS FROM ALUMINIUM ALLOYS | 2012 |
|
RU2482949C1 |
WEAR-RESISTANT COATING PRODUCTION METHOD | 2012 |
|
RU2484185C1 |
ELECTROCHEMICAL PROCESS OF COATING METALLIC PARTS | 2012 |
|
RU2483145C1 |
METHOD FOR MICRO-ARC OXIDATION | 2008 |
|
RU2389830C2 |
METHOD OF ELECTROCHEMICAL OXIDATION OF COATINGS ON VALVE METALS OR ALLOYS | 2019 |
|
RU2718820C1 |
PROCEDURE FOR STRENGTHENING SEATS OF VALVES OF INTERNAL COMBUSTION ENGINES OUT OF ALUMINIUM ALLOY | 2008 |
|
RU2390587C2 |
METHOD FOR OBTAINING COMPOSITE COATINGS ON VALVE METALS AND THEIR ALLOYS | 2022 |
|
RU2787330C1 |
ELECTROLYTIC METHOD FOR APPLICATION OF PROTECTIVE AND ELECTROINSULATING COATS | 2008 |
|
RU2367727C1 |
METHOD OF ALUMINIUM AND ITS ALLOYS ANODIZING | 1992 |
|
RU2039133C1 |
Authors
Dates
2015-02-10—Published
2013-11-21—Filed