FIELD: electricity.
SUBSTANCE: mineral activating agent contains (% by weight): shungite powder 90-99, water-soluble tertiary amine (pH 8-10) 10-1.
EFFECT: improved electrical performance for protected facilities by stabilising the weight of the activating agent, polarisation potential and transient resistance at the phase boundary of the ground and the activating agent, reduced current-spreading resistance.
3 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ANODE ACTIVATOR OF ELECTROCHEMICAL CORROSION PROTECTION OF UNDERGROUND STRUCTURES (VARIANTS) | 2016 |
|
RU2650021C1 |
BIO-CORROSION INHIBITOR FOR METAL OBJECT | 2019 |
|
RU2717415C1 |
APPLIANCE FOR UNDERGROUND ASSEMBLED STEEL SECTIONS CATHODIC PROTECTION | 2016 |
|
RU2632056C1 |
PLANT LIFE ELECTROSTIMULATION DEVICE | 2019 |
|
RU2717035C1 |
ANODE GROUNDING ELECTRODE, COMPOSITION OF ANODE GROUND ELECTRODE AND METHOD FOR ITS PRODUCTION | 1996 |
|
RU2071510C1 |
COKE-MINERAL PROMOTER OF ELECTROCHEMICAL CORROSION PROTECTION ANODES | 1999 |
|
RU2161353C1 |
COMPOSITION FOR ANODE GROUND ELECTRODE | 1995 |
|
RU2084029C1 |
ANODE SPACE FILLER | 2014 |
|
RU2585490C1 |
ANODE GROUNDING | 1991 |
|
RU2033476C1 |
ANODE EARTHING ELECTRODE | 2013 |
|
RU2542867C2 |
Authors
Dates
2015-08-10—Published
2014-05-22—Filed