FIELD: agriculture.
SUBSTANCE: plates with two holes are punched. The one-sided working ends of the plate are reinforced by hard facing. Before reinforcement along the perimeter of one or both ends of one side of the plate the openings or slots are made at a depth of 1/2-1/3 thickness of the hammer at a distance of 2.0-2.5 mm from its edges.
EFFECT: increase in the lifetime of the hammers.
4 dwg
Title | Year | Author | Number |
---|---|---|---|
PLATY BEATER FOR FODDER GRINDER | 2008 |
|
RU2379109C1 |
METHOD FOR INDUCTION SURFACING OF ITEMS OF END SURFACES | 2015 |
|
RU2631565C2 |
METHOD OF SURFACE HARDENING OF STEEL PART CONTAINING DEAD-END CAVITIES | 2014 |
|
RU2569872C1 |
TAPE FOR HARDENING OF PARTS BY INDUCTION HARD-FACING WITH UNILATERAL ADHESION AND METHOD OF INDUCTION HARD-FACING | 2013 |
|
RU2548338C2 |
METHOD OF INDUCTION BUILD-UP OF HIGH ALLOYED CHROMOUS CAST IRONS | 2014 |
|
RU2568036C2 |
METHOD FOR INDUCTION SURFACING OF IRON-BASED MAGNETIC ALLOYS AND INDUCTION-CHANNEL FURNACE FOR INDUCTION SURFACING OF IRON-BASED MAGNETIC ALLOYS | 2021 |
|
RU2791023C1 |
METHOD OF PRODUCING MOULDED STEEL PART | 2015 |
|
RU2622503C2 |
METHOD FOR MATERIALS WEAR RESISTANCE DETERMINATION OF THE AGRICALTURAL MACHINES OPERATING BODIES HARDENING COATINGS | 2016 |
|
RU2618604C1 |
METHOD OF MANUFACTURING THE KNIFE OF THE STRAW SHREDDER | 2017 |
|
RU2665483C1 |
METHOD OF INDUCTION WELD DEPOSITION OF WEAR-RESISTANT COATING | 2014 |
|
RU2561560C1 |
Authors
Dates
2015-09-20—Published
2014-07-03—Filed