FIELD: metallurgy.
SUBSTANCE: heat-resistant cord along the weld surface is mounted or glued. The facing charge is loaded on the surface limited with the cord. Surfacing is carried out by high-frequency generator operating at 66 kHz frequency. Heat-resistant asbestos cord is prepared by soaking in glass liquid solution, dried and hold in 5% alcohol rosin solution.
EFFECT: reducing the complexity of item and charge preparation and surfacing process.
2 cl, 5 dwg, 1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF INDUCTION BUILD-UP OF HIGH ALLOYED CHROMOUS CAST IRONS | 2014 |
|
RU2568036C2 |
METHOD OF SURFACE HARDENING OF STEEL PART CONTAINING DEAD-END CAVITIES | 2014 |
|
RU2569872C1 |
TAPE FOR HARDENING OF PARTS BY INDUCTION HARD-FACING WITH UNILATERAL ADHESION AND METHOD OF INDUCTION HARD-FACING | 2013 |
|
RU2548338C2 |
METHOD OF INDUCTION WELD DEPOSITION OF WEAR-RESISTANT COATING | 2014 |
|
RU2561560C1 |
POWDER THERMO-REACTIVE CHARGE FOR INDUCTION WELDING OF SOLID ALLOY | 2015 |
|
RU2637736C2 |
METHOD FOR INDUCTION SURFACING OF IRON-BASED MAGNETIC ALLOYS AND INDUCTION-CHANNEL FURNACE FOR INDUCTION SURFACING OF IRON-BASED MAGNETIC ALLOYS | 2021 |
|
RU2791023C1 |
METHOD OF PRODUCTION OF PLATE HAMMER OF FEED GRINDER | 2014 |
|
RU2563696C1 |
CHARGE FOR INDUCTION SURFACING OF WEAR-RESISTANT ALLOY | 2020 |
|
RU2755913C1 |
METHOD OF DETERMINING PROCESS TEMPERATURE OF CHARGE MELTING DURING INDUCTION SURFACING | 2019 |
|
RU2714522C1 |
METHOD FOR DETERMINING THE MELTING POINT OF A POWDER MIXTURE | 2022 |
|
RU2785101C1 |
Authors
Dates
2017-09-25—Published
2015-05-18—Filed